Graphite raw MATERIAL (needle coke or petroleum coke) was mixed with binder for air flow milling (crushing) and PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC removal of iron. According to the different products, graphite raw materials and adhesives (graphitization) are mixed in different proportions, the mixing ratio is 100 :(5~20), the material is transferred to the hopper through the vacuum feeding machine, and then the hopper is put into the air flow mill for air grinding powder, and the raw materials with the particle size of 5~10mm are ground to 5-10 microns.
After air flow grinding, the MATERIAL with required particle size is collected by cyclone dust collector with a dust collection rate of about 80%. The MATERIAL is entered into PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC removal, and the tail gas is filtered and discharged by the filter element filter with a dust removal efficiency greater than 99%. The filter element is made of filter cloth with pore size less than 0.2 micron, which can intercept all dust above 0.2 micron. The fan controls the whole system under negative pressure.
Granulation is a key part of Delanium graphite processing. It is divided into pyrolysis process, ball milling and PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC screening process. Difference: At present, there is little difference in particle size screening among enterprises, mainly reflected in the details and cost.
Contact: DELLA
Mob: +86-13929907491
Адрес : No.9, Factory 2, Shijin Industry Park, Shishan Town, Nanhai District, Foshan City, Guangdong, China
Тел. : +86 -13929907491
Эл. адрес : sales@ptmsmagnet.com
Веб-сайт : https://www.dellamagnet.com